TM-2261 Transparent Acrylic Acidum Hot Mounting Powder
depictio producti
TM 2261 cum cerussa pellucet appearance.
depictio producti
TM 2261 cum cerussa pellucet appearance.
Features
Features: Transparens et valde clear.allows facile specimen observationis.
Technical Parameters
| Descriptio | Perspicuus |
| Components | Pulvis albus |
| Tempus calor | 6-8 min |
| Tempus refrigerandum | 7-10 min |
| Celeritas refrigerandum | low |
| Pressura | 100-150 bar |
| Calor temperatus | 160-180 °C |
| duritia | 85-87 Shore D |
Informationes iussis
| Ordo nullus: | Descriptio | sarcina |
| 02.01.140 | Pulvis albus | 1kg |
| 02.01.144 | Pulvis albus | 4kg |
| 02.01.145 | Pulvis albus | 20 kg |
Similia Products
| Troianus | Struers | Buehler | ATM |
| TM-2261 | ClaroFast | TransOptic | Thermoplast |